Basit öğe kaydını göster

dc.contributor.authorAteş, Sabit Melih
dc.contributor.authorÇağlar, İpek
dc.contributor.authorDuymuş, Zeynep Yeşil
dc.date.accessioned2023-02-22T11:12:24Z
dc.date.available2023-02-22T11:12:24Z
dc.date.issued2021en_US
dc.identifier.citationAteş, S.M., Çağlar, İ. & Duymuş, Z.Y. (2021). Farklı Bağlayıcı Ajanlar Uygulanmış Lazer Sinterize Kobalt-Krom Alaşımına Kompozit Bağlantısının İncelenmesi. Türkiye Klinikleri Diş Hekimliği Bilimleri Dergisi, 27(1), 58-64. http://doi.org/10.5336/dentalsci.2020-74389en_US
dc.identifier.issn2146-8966
dc.identifier.urihttp://doi.org/10.5336/dentalsci.2020-74389
dc.identifier.urihttps://hdl.handle.net/11436/7676
dc.description.abstractAmaç: Bu çalışmanın amacı 4 farklı bağlayıcı ajan uygulanmış lazer sinterize kobalt-krom (Co-Cr) alaşımına akışkan kompozitin makaslama bağlantı dayanımını incelemektir. Gereç ve Yöntemler: Toplam 100 adet lazer sinterize Co-Cr örnek üretildi ve uygulanacak bağlayıcı ajana göre 5 farklı test grubuna ayrıldı (n = 20): Grup (1) kontrol, bağlayıcı ajan uygulanmadı; Grup (2) Alloy Primer (Kuraray Dental, Tokyo, Japonya) uygulandı; Grup (3) Z-Prime Plus (Bisco Inc., IL, A.B.D) uygulandı; Grup (4) Gluma Bond (Heraeus Kulzer GmbH, Hanau, Almanya) uygulandı ve Grup (5) Single Bond Universal (3M Espe GmbH, Neuss, Almanya) uygulandı. Bağlayıcı ajan uygulamasından sonra Co-Cr yüzeyler üzerine akışkan kompozit uygulandı. Örnekler 37°C’deki distile su içinde 24 saat bekletildikten sonra termalsiklusa (5ºC ve 55ºC, 30 saniye döngü süresi, 5000 siklus) tabi tutuldu ve universal test cihazında makaslama bağlantı dayanımı testi yapıldı. Örneklerde oluşan başarısızlık tipleri stereomikroskop ile incelendi. Elde edilen verilerin istatistiksel analizi tek yönlü ANOVA ile yapıldı ve sonrasında Tukey testi kullanılarak gruplara ait ortalama bağlantı dayanımı değerleri karşılaştırıldı (α=0.05). Bulgular: Çalışmada kullanılan tüm bağlayıcı ajanlar akışkan kompozit rezinin bağlantı dayanımı değerlerini istatistiksel olarak anlamlı olacak şekilde arttırmıştır. En yüksek bağlantı dayanımı değeri Single Bond Universal uygulanan grupta (18.2 ± 2.1 MPa), en düşük bağlantı dayanımı değeri kontrol grubunda bulundu (5.3± 0.8 MPa). Sonuç: Çalışmada kullanılan 4 farklı bağlayıcı ajanın akışkan kompozitin lazer sinterize Co-Cr alaşımına bağlantısında etkili olduğu, bununla birlikte Single Bond Universal uygulamasının bağlantı dayanımını daha iyi geliştirebileceği sonucuna varılmıştır.en_US
dc.description.abstractObjective: The aim of this study was to examine the shear bond strength of a flowable composite resin to laser sintered cobalt-chromium (Co-Cr) alloy, using 4 different adhesives. Material and Methods: A total of 100 laser sintered Co-Cr samples were fabricated and divided into 5 test groups (n = 20) according to the adhesive used: group (1) control, no treatment; group (2) Alloy Primer (Kuraray Dental, Tokyo, Japan) application; group (3) Z-Prime Plus (Bisco Inc., IL, USA) application; group (4) Gluma Bond (Heraeus Kulzer GmbH, Hanau, Germany) application and group (5) Single Bond Universal (3M Espe GmbH, Neuss, Germany) application. After adhesive applications, flowable composite resin was applied to the Co-Cr surfaces. After storing in distilled water at 37°C for 24 hours, specimens were thermally cycled (5ºC and 55ºC, 30 second dwell time, 5000 cycles) and tested in shear mode in an universal testing machine. The failure modes were determined with a stereomicroscope. Mean bond strength values were analyzed by using One-way ANOVA followed by Tukey’s multiple comparison tests (α=0.05). Results: All tested adhesives significantly increased the bond strength values of flowable composite resin. The highest bond strength values were observed in the Single Bond Universal application group (18.2 ± 2.1 MPa), while the lowest values were observed in the control group (5.3 ± 0.8 MPa). Conclusion: Application of each of the four adhesives was effective for bonding of flowable composite to laser sintered Co-Cr alloy, however Single Bond Universal application may result in improved bond strength values.en_US
dc.language.isoturen_US
dc.publisherTürkiye Klinikleri Yayınevien_US
dc.rightsinfo:eu-repo/semantics/openAccessen_US
dc.subjectBağlantı ajanlarıen_US
dc.subjectDiş protez tamirien_US
dc.subjectKrom-kobalt alaşımlarıen_US
dc.subjectBonding agentsen_US
dc.subjectChromium-cobalt alloysen_US
dc.subjectDental prosthesis repairen_US
dc.titleFarklı bağlayıcı ajanlar uygulanmış lazer sinterize kobalt-krom alaşımına kompozit bağlantısının incelenmesien_US
dc.title.alternativeInvestigation of composite bonding to laser-sintered cobalt-chromium alloy treated with different adhesive agentsen_US
dc.typearticleen_US
dc.contributor.departmentRTEÜ, Diş Hekimliği Fakültesi, Klinik Bilimler Bölümüen_US
dc.contributor.institutionauthorAteş, Sabit Melih
dc.contributor.institutionauthorÇağlar, İpek
dc.contributor.institutionauthorDuymuş, Zeynep Yeşil
dc.identifier.doi10.5336/dentalsci.2020-74389en_US
dc.identifier.volume27en_US
dc.identifier.issue1en_US
dc.identifier.startpage58en_US
dc.identifier.endpage64en_US
dc.relation.journalTürkiye Klinikleri Diş Hekimliği Bilimleri Dergisien_US
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanıen_US


Bu öğenin dosyaları:

Thumbnail

Bu öğe aşağıdaki koleksiyon(lar)da görünmektedir.

Basit öğe kaydını göster