Effect of strontium additions on the microstructural and mechanical properties of Al-17Si-4Cu-0.6Mg-3Zn (B390+2 wt%Zn) alloy
(Springer, 2022)
One Al-17Si-4Cu-0.6Mg-3Zn (B390 + 2 wt%Zn) alloy and five B390 + 2 wt% Zn-Sr alloys were produced by permanent mold casting method. Microstructural evaluations were carried out with microscopic techniques. The phases of ...
Effect of different zinc contents on the structural, mechanical and tribological properties of EN AC-48100 (Al-17Si-4Cu-Mg) Alloy
(Gazi Univ, Fac Engineering Architecture, 2020)
In this study, Al-17Si-4Cu-0.6Mg-0.2Ti which is based of the EN AC-48100 alloy, Al-17Si-4Cu-0.6Mg0.2Ti-1Zn, Al-17Si-4Cu-0.6Mg-0.2Ti-2Zn, Al- 17Si-4Cu-0.6Mg-0.2Ti-3Zn, Al-17Si-4Cu-0.6Mg-0.2Ti-4Zn and Al-17Si-4Cu-0.6Mg-0.2Ti-5Zn ...