Effect of grain refinement with titanium on the microstructure, mechanical and corrosion properties of Al-25Zn alloy
(Gazi Univ, Fac Engineering Architecture, 2020)
In this study, one binary Al-25n alloys and eleven ternary aluminum-zinc-titanium alloys, Al-25Zn-0.01Ti, Al-25Zn-0.03Ti, Al-25Zn-0.04Ti, Al-25Zn-0.05Ti, Al-25Zn-0.075Ti, Al-25Zn-0.1Ti, Al-25Zn-0.2Ti, Al-25Zn-0.4Ti, ...
Effect of zinc content and cutting tool coating on the machinability of the Al-(5-35) Zn alloys
(Korean Inst Metals Materials, 2020)
In this study, Al-5Zn, Al-15Zn, Al-25Zn and Al-35Zn alloys containing 5, 15, 25 and 35 wt% Zn, respectively were produced by permanent mold casting. Their microstructures and mechanical properties were investigated using ...
Effect of different zinc contents on the structural, mechanical and tribological properties of EN AC-48100 (Al-17Si-4Cu-Mg) Alloy
(Gazi Univ, Fac Engineering Architecture, 2020)
In this study, Al-17Si-4Cu-0.6Mg-0.2Ti which is based of the EN AC-48100 alloy, Al-17Si-4Cu-0.6Mg0.2Ti-1Zn, Al-17Si-4Cu-0.6Mg-0.2Ti-2Zn, Al- 17Si-4Cu-0.6Mg-0.2Ti-3Zn, Al-17Si-4Cu-0.6Mg-0.2Ti-4Zn and Al-17Si-4Cu-0.6Mg-0.2Ti-5Zn ...
Effects of titanium addition on structural, mechanical, tribological, and corrosion properties of Al-25Zn-3Cu and Al-25Zn-3Cu-3Si alloys
(Elsevier, 2020)
To investigate the effect of grain refinement on the material properties of recently developed Al-25Zn-3Cu based alloys, Al-25Zn-3Cu, Al-25Zn-3Cu-0.01Ti, Al-25Zn-3Cu-3Si and Al-25Zn-3Cu-3Si-0.01Ti alloys were produced by ...
The effect of solid boriding time on the structure, hardness and corrosion properties of AISI 5140 steel
(Maik Nauka/Interperiodica/Springer, 2020)
In this study, AISI 5140 steel samples were borided in an electrical furnace at a temperature of 950 degrees C for 4, 6 and 8 h. Structural examinations, hardness measurement and corrosion tests were performed to determine ...
Effect of strontium on the microstructure, mechanical, and tribological properties of the Zn-40Al-2Cu alloy
(Springer, 2023)
Zn-40Al-2Cu and Zn-40Al-2Cu-0.1Sr alloys were produced by permanent mold casting method. The microstructure, mechanical properties and wear resistance of the produced alloys were investigated. Microstructural examinations ...
Performance evaluation of different carbide inserts in turning of newly developed Al-12Si-0.1Sr alloyLeistungsbewertung verschiedener Hartmetalleinsatze beim Drehen einer neu entwickelten Al-12Si-0.1Sr-Legierung
(Wiley, 2023)
An Al-12Si-0.1Sr alloy ingot was manufactured using a permanent mold casting technique. The microstructure and mechanical properties of this alloy were researched. Effects of different cutting conditions (cutting speed-V: ...
Effect of isothermal treatment on mechanical and tribological properties of alloy Zn – 40% Al – 2% Cu – 2% Si
(Springer, 2023)
The effect of isothermal exposure at temperatures from 100°C to 250°C for 8 hours on the structure, mechanical and tribological properties of the Zn – 40% Al – 2% Cu – 2% Si alloy produced by chill casting is studied. The ...
Mechanical properties of Al-9Si-0.6Mg-0.1Sr alloy processed by successive hot and cold multi-directional forging