dc.identifier.citationGuner, N. U., Kutuk, S., & Kutuk-Sert, T. (2025). Role of calcination process of natural colemanite powder on compressive strength property of concrete. Heliyon, 11(1), e41264. https://doi.org/10.1016/j.heliyon.2024.e41264en_US
dc.identifier.issn2405-8440
dc.identifier.urihttps://doi.org/10.1016/j.heliyon.2024.e41264
dc.identifier.urihttps://hdl.handle.net/11436/9859
dc.description.abstractThe use of boron minerals as an additive is important in terms of reducing CO2 emissions and providing input to the economy. Sustainable natural colemanite was subjected to calcination at 550 °C in order to concentrate the amount of B2O3. For the characterization of calcined mineral, XRD, TGA/DTA, and B2O3 component tests were carried out. It was observed that the structure of natural colemanite changed, and the B2O3 value heightened by 11 %. Then, natural and calcined minerals were added to the concrete mixture in proportions of 1.25 %, 2.5 %, 5 %, 7.5 %, 10 %, 12.5 %, and 15 % by weight. Ultrasonic pulse velocity, Schmidt hardness, and compressive strength tests were fulfilled. In the samples with natural additives, the lowest compressive strength was 32 MPa for the reference sample, whereas the highest strength was 44 MPa for the 10 % natural colemanite sample. In other words, the compressive strength increased by 39 %. In the samples with calcined additives, the highest compressive strength was 30 MPa for the 2.5 % calcined colemanite sample; that is, it improved by 24 %. It is realized that the cement can be saved since high strength can be obtained in concrete with natural and calcined colemanite additiveen_US
dc.language.isoengen_US
dc.publisherElsevieren_US
dc.rightsinfo:eu-repo/semantics/openAccessen_US
dc.subjectBoronen_US
dc.subjectCalcinationen_US
dc.subjectCO2 emissionsen_US
dc.subjectCompressive strengthen_US
dc.subjectConcreteen_US
dc.subjectMineral additiveen_US
dc.titleRole of calcination process of natural colemanite powder on compressive strength property of concreteen_US
dc.typearticleen_US
dc.contributor.departmentRTEÜ, Mühendislik ve Mimarlık Fakültesi, İnşaat Mühendisliği Bölümüen_US
dc.contributor.institutionauthorGüner, Nihat Utku
dc.contributor.institutionauthorKütük, Sezai
dc.contributor.institutionauthorKütük Sert, Tuba
dc.identifier.doi10.1016/j.heliyon.2024.e41264en_US
dc.identifier.volume11en_US
dc.identifier.issue1en_US
dc.identifier.startpagee41264en_US
dc.relation.journalHeliyonen_US
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanıen_US


Bu öğenin dosyaları:

Bu öğe aşağıdaki koleksiyon(lar)da görünmektedir.

Basit öğe kaydını göster