Basit öğe kaydını göster

dc.contributor.authorHekimoğlu, Ali Paşa
dc.contributor.authorHacıosmanoğlu, Murat
dc.contributor.authorBaki, Muzaffer
dc.date.accessioned2020-12-19T19:35:21Z
dc.date.available2020-12-19T19:35:21Z
dc.date.issued2020
dc.identifier.citationHekimoğlu, A:P., Hacıosmanoğlu, M. & Baki, M. (2020). Effect of different zinc contents on the structural, mechanical and tribological properties of EN AC-48100 (Al-17Si-4Cu-Mg) Alloy. Journal of the Faculty of Engineering and Architecture of Gazi University, 35(4), 1799-1814. https://doi.org/10.17341/gazimmfd.602161en_US
dc.identifier.issn1300-1884
dc.identifier.issn1304-4915
dc.identifier.urihttps://doi.org/10.17341/gazimmfd.602161
dc.identifier.urihttps://hdl.handle.net/11436/1275
dc.descriptionWOS: 000552077900008en_US
dc.description.abstractIn this study, Al-17Si-4Cu-0.6Mg-0.2Ti which is based of the EN AC-48100 alloy, Al-17Si-4Cu-0.6Mg0.2Ti-1Zn, Al-17Si-4Cu-0.6Mg-0.2Ti-2Zn, Al- 17Si-4Cu-0.6Mg-0.2Ti-3Zn, Al-17Si-4Cu-0.6Mg-0.2Ti-4Zn and Al-17Si-4Cu-0.6Mg-0.2Ti-5Zn alloys were produced by permanent mold casting method. Chemical composition of the produced alloys was determined by the spark optical emission spectrometer method. the microstructures of the alloys were examined by optical and scanning electron microscopy. the hardness and microhardness of the alloys were determined by Brinell and Vickers measurement methods, respectively, and their mechanical properties were determined by tensile tests performed by a universal test machine. It was observed that the microstructure of the Al-17Si-4Cu-0.6Mg-0.2Ti-(0-5) Zn alloys consisted of aluminum-rich alpha, eutectic Al-Si, primary silicon, copper-rich theta (CuAl2), Mg2Si and pi phases. It was also observed that zinc additions did not lead to a new phase formation in the Al-17Si-4Cu-0.6Mg-0.2Ti alloy. the hardness of the produced alloys increased with increasing zinc content, but yield and tensile strength and wear resistance increased up to 3% zinc content and decreased after this ratio. Smearing layers, fine scratches and peeling occurred are seen on the surfaces of the wear samples. the morphology of the wear particles collected after wear tests did not show significant change with the zinc content. the results obtained from the mechanical and tribological tests of the produced alloys were discussed in terms of the microstructural features of the alloys.en_US
dc.language.isoturen_US
dc.publisherGazi Univ, Fac Engineering Architectureen_US
dc.rightsinfo:eu-repo/semantics/openAccessen_US
dc.subjectAl-17Si based alloysen_US
dc.subjectMicrostructureen_US
dc.subjectMechanical propertiesen_US
dc.subjectFractureen_US
dc.subjectFriction-wearen_US
dc.titleEffect of different zinc contents on the structural, mechanical and tribological properties of EN AC-48100 (Al-17Si-4Cu-Mg) Alloyen_US
dc.typearticleen_US
dc.contributor.departmentRTEÜ, Mühendislik ve Mimarlık Fakültesi, Makine Mühendisliği Bölümüen_US
dc.contributor.institutionauthorHekimoğlu, Ali Paşa
dc.contributor.institutionauthorHacıosmanoğlu, Murat
dc.identifier.doi10.17341/gazimmfd.602161
dc.identifier.volume35en_US
dc.identifier.issue4en_US
dc.identifier.startpage1799en_US
dc.identifier.endpage1814en_US
dc.ri.editoaen_US
dc.relation.journalJournal of the Faculty of Engineering and Architecture of Gazi Universityen_US
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanıen_US


Bu öğenin dosyaları:

Thumbnail

Bu öğe aşağıdaki koleksiyon(lar)da görünmektedir.

Basit öğe kaydını göster