dc.identifier.citationUsta Kutlu, I., Yanikoğlu, N. D., Kul, E., Duymuş, Z. Y., & Sağsöz, N. P. (2016). Effect of sealer coating and storage methods on the surface roughness of soft liners. The Journal of prosthetic dentistry, 115(3), 371–376. https://doi.org/10.1016/j.prosdent.2015.10.004en_US
dc.identifier.issn0022-3913
dc.identifier.issn1097-6841
dc.identifier.urihttps://hdl.handle.net/11436/2567
dc.descriptionkutlu, ilknur usta/0000-0001-7532-7954en_US
dc.descriptionWOS: 000371280600021en_US
dc.descriptionPubMed: 26723099en_US
dc.description.abstractStatement of problem. A soft lining is applied under a removable prosthesis for various reasons. the porosity of the lining material may increase colonization by microorganisms and cause tissue inflammation. Purpose. the purpose of this in vitro study was to evaluate the effect of sealer coating on the surface roughness of soft lining materials under 4 different conditions. Material and methods. A total of 125 specimens were prepared. One high-temperature silicone based soft lining material and 2 room-temperature-polymerized soft lining materials (1 silicone based and 1 methacrylate-based) were used. Twenty-five specimens of each room-temperature soft lining material were coated with 2 layers of surface sealer. Additionally, 5 specimens of each material were stored in either distilled water, Coca-Cola, denture cleanser, saliva, or air. the surface roughness was measured at baseline and after 1, 7, 14, and 28 days. Surface roughness values were analyzed with repeated measures analysis of variance, and the Bonferroni multiple comparison test was performed using time-dependent groups and storage methods. Results. in the time-dependent groups, methacrylate-based sealer-coated soft liners exhibited a significant increase in roughness (1.74-2.09 m, P<.001), and silicone-based sealer-coated soft liners exhibited a decrease in roughness, but it was not significant (2.16-2.02 m, P>.05). Therefore, the sealer coating was not effective in reducing surface roughness. Among the time dependent storage methods, the denture cleanser exhibited an almost significant increase in roughness (1.83-1.99 p.m, P=.054). Coca-Cola and artificial saliva did not show a significant difference (P>.05). However, a significant decrease in roughness was found with distilled water (P=.02) and air (P<.001). Conclusions. Statistically significant differences in surface roughness were found among the different types of soft liners. the sealer coating had no significant effect, and denture cleanser slightly increased the surface roughness. Contrary to expectations, the roughness did not increase in all groups over time.en_US
dc.language.isoengen_US
dc.publisherMosby-Elsevieren_US
dc.rightsinfo:eu-repo/semantics/closedAccessen_US
dc.subjectLining materialsen_US
dc.subjectCandida-albicansen_US
dc.subjectDenture cleansersen_US
dc.subjectTıssue conditionersen_US
dc.subjectBond strengthen_US
dc.titleEffect of sealer coating and storage methods on the surface roughness of soft linersen_US
dc.typearticleen_US
dc.contributor.departmentRTEÜ, Diş Hekimliği Fakültesi, Klinik Bilimler Bölümüen_US
dc.contributor.institutionauthorDuymuş, Zeynep Yeşil
dc.identifier.volume115en_US
dc.identifier.issue3en_US
dc.identifier.startpage371en_US
dc.identifier.endpage376en_US
dc.relation.journalJournal of Prosthetic Dentistryen_US
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanıen_US


Bu öğenin dosyaları:

Thumbnail

Bu öğe aşağıdaki koleksiyon(lar)da görünmektedir.

Basit öğe kaydını göster