Peel strength of denture liner to PMMA and polyamide: laser versus air-abrasion

Göster/ Aç
Erişim
info:eu-repo/semantics/openAccessTarih
2013Yazar
Korkmaz, Fatih MehmetBağış, Bora
Özcan, Mutlu
Durkan, Rukiye
Turgut, Sedanur
Ateş, Sabit Melih
Üst veri
Tüm öğe kaydını gösterKünye
Korkmaz, F.M., Bagis, B., Ozcan, M., Durkan, R., Turgut, S., Ates, S.M., (2013). Peel strength of denture liner to PMMA and polyamide: laser versus air-abrasion. Journal of Advanced Prosthodontics, 5(3), 287-295.https://doi.org/10.4047/jap.2013.5.3.287Özet
PURPOSE. This study investigated the effect of laser parameters and air-abrasion on the peel strength of silicon-based soft denture liner to different denture resins. MATERIALS AND METHODS. Specimens (N=180) were prepared out of three different denture base resins (Rodex, cross-linked denture base acrylic resin; Paladent, heat-cured acrylic resin; Deflex, Polyamide resin) (75 mm x 25 mm x 3 mm). A silicon-based soft denture liner (Molloplast B) was applied to the denture resins after the following conditioning methods: a) Air-abrasion (50 pm), b) Er,Cr:YSGG laser (Waterlase MD Turbo, Biolase Technology) at 2 W-20 Hz, c) Er,Cr:YSGG laser at 2 W-30 Hz, d) Er,Cr:YSGG laser at 3 W-20 Hz, e) Er,Cr:YSGG laser at 3 W-30 Hz. Non-conditioned group acted as the control group. Peel test was performed in a universal testing machine. Failure modes were evaluated visually. Data were analyzed using two-way ANOVA and Tukey's test (alpha=.05). RESULTS. Denture liner tested showed increased peel strength after laser treatment with different parameters (3.9 +/- 0.4 - 5.58 +/- 0.6 MPa) compared to the control (3.64 +/- 0.5 - 4.58 +/- 0.5 MPa) and air-abraded groups (3.1 +/- 0.6 - 4.46 +/- 0.3 MPa), but the results were not statistically significant except for Paladent, with the pretreatment of Er,Cr:YSGG laser at 3 W-20 Hz. Polyamide resin after air-abrasion showed significantly lower peel strength than those of other groups (3.1 +/- 0.6 MPa). CONCLUSION. Heat-cured acrylic resin, PMMA, may benefit from Er,Cr:YSGG laser treatment at 3 W-20 Hz irradiation. Air-abrasion of polyamide resins should be avoided not to impair their peel bond strengths to silicon-based soft denture liners.