dc.identifier.citationÇağlar, B., Afşin, B., Eren, E., Tabak, A., Çırak, Ç. & Çubuk, O. (2010). The spectral, structral and thermal characterizations of dimethyl sulphoxide, pyridine, ethanolamine and N-methyl formamide intercalated kaolinites. Zeitschrift fur Naturforschung - Section A Journal of Physical Sciences, 65(11), 1009-1019. https://doi.org/10.1515/zna-2010-1111en_US
dc.identifier.issn0932-0784
dc.identifier.urihttps://doi.org/10.1515/zna-2010-1111
dc.identifier.urihttps://hdl.handle.net/11436/3816
dc.description.abstractThe intercalation of dimethyl sulphoxide (DMSO), pyridine (Py), ethanolamine (Ea), and Nmethyl formamide (NMF) molecules into the kaolinite interlayers led to an appreciable decrease of 3697 cm-1 of the hydroxyl band. The appearance of the peaks at 3662, 3541, and 3504 cm-1 proved that the DMSO species are intercalated between the kaolinite layers through forming H-bonds with internal-surface hydroxyl groups. The intensities of the 942 and 796 cm-1 bending peaks arising from inner-surface hydroxyls decreased and new vibrational features appeared due to the intercalation of the guest species. The d001 value of pure kaolinite was found at 7.18 Å, and the d001 values were seen at 11.26, 11.62, 10.77, and 10.67 Å for kaolinite-dimethyl sulphoxide (K-DMSO), kaolinite-pyridine (K-Py), kaolinite-ethanolamine (K-EA), and kaolinite-N-methyl formamide (K-NMF) composites, respectively. The endothermic differential thermal analysis (DTA) peaks at a temperature of 108 - 334°C reflected the changes in the physicochemical properties of the intercalated species. The thermal stability increase followed the order of K-Py<K-NMF<K-Ea<K-DMSO. Based on the thermal analysis data, the intercalation ratios of the composites above were determined as 80.0, 40.0, 81.6, and 82.0%, respectively. The specific surface areas are affected by the intercalation geometry of the composites within the gallery spacing. The surface areas of the K-DMSO, K-Py, and K-EA complexes increased whereas the surface area of K-NMF decreased with respect to that of untreated kaolinite. © 2010 Verlag der Zeitschrift für Naturforschung, Tübingen.en_US
dc.language.isoengen_US
dc.publisherVerlag der Zeitschrift fur Naturforschungen_US
dc.rightsinfo:eu-repo/semantics/openAccessen_US
dc.subjectInner-surface hydroxylsen_US
dc.subjectIntercalationen_US
dc.subjectKaoliniteen_US
dc.subjectThermal analysisen_US
dc.subjectXRDen_US
dc.titleThe spectral, structral and thermal characterizations of dimethyl sulphoxide, pyridine, ethanolamine and N-methyl formamide intercalated kaolinitesen_US
dc.typearticleen_US
dc.contributor.departmentRTEÜ, Fen - Edebiyat Fakültesi, Kimya Bölümüen_US
dc.contributor.institutionauthorTabak, Ahmet
dc.identifier.doi10.1515/zna-2010-1111
dc.identifier.volume65en_US
dc.identifier.issue11en_US
dc.identifier.startpage1009en_US
dc.identifier.endpage1019en_US
dc.relation.journalZeitschrift fur Naturforschung - Section A Journal of Physical Sciencesen_US
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanıen_US


Bu öğenin dosyaları:

Bu öğe aşağıdaki koleksiyon(lar)da görünmektedir.

Basit öğe kaydını göster