Effect of strontium additions on the microstructural and mechanical properties of Al-17Si-4Cu-0.6Mg-3Zn (B390+2 wt%Zn) alloy
(Springer, 2022)
One Al-17Si-4Cu-0.6Mg-3Zn (B390 + 2 wt%Zn) alloy and five B390 + 2 wt% Zn-Sr alloys were produced by permanent mold casting method. Microstructural evaluations were carried out with microscopic techniques. The phases of ...
Effect of grain refinement with titanium on the microstructure, mechanical and corrosion properties of Al-25Zn alloy
(Gazi Univ, Fac Engineering Architecture, 2020)
In this study, one binary Al-25n alloys and eleven ternary aluminum-zinc-titanium alloys, Al-25Zn-0.01Ti, Al-25Zn-0.03Ti, Al-25Zn-0.04Ti, Al-25Zn-0.05Ti, Al-25Zn-0.075Ti, Al-25Zn-0.1Ti, Al-25Zn-0.2Ti, Al-25Zn-0.4Ti, ...