Ara
Toplam kayıt 19, listelenen: 1-10
Effects of contact pressure and sliding speed on the unlubricated friction and wear properties of Zn-15Al-3Cu-1Si alloy
(Taylor & Francis Inc, 2016)
The unlubricated friction and wear properties of Zn-15Al-3Cu-1Si alloy were studied over a range of contact pressure (1-5 MPa) and sliding speed (0.5-2.5 ms(-1)) for a sliding distance of 2,500m using a block-on-disc type ...
Effect of heat treatment on mechanical and wear properties of Zn-40Al-2Cu-2Si alloy
(Elsevier, 2021)
In order to determine the effect of heat treatment on the mechanical and wear properties of Zn-40Al-2Cu-2Si alloy, different heat treatments including homogenization followed by air-cooling (H1), homogenization followed ...
Effect of strontium additions on the microstructural and mechanical properties of Al-17Si-4Cu-0.6Mg-3Zn (B390+2 wt%Zn) alloy
(Springer, 2022)
One Al-17Si-4Cu-0.6Mg-3Zn (B390 + 2 wt%Zn) alloy and five B390 + 2 wt% Zn-Sr alloys were produced by permanent mold casting method. Microstructural evaluations were carried out with microscopic techniques. The phases of ...
Effect of arc re-melting on microstructure, mechanical and tribological properties of commercial 390A alloy
(Elsevier, 2021)
To investigate the effect of the arc re-melting on the microstructure, mechanical and tribological properties of the 390A alloy, its ingot produced by the conventional induction melting method was subjected to the arc ...
Kokil kalıba döküm yöntemi ile üretilmiş Al-12Si-(0,02-1)Sr alaşımlarının CVD-TiCN/Al2O3/TiN kaplamalı kesici uç ile tornada işlenmesinde kesme kuvveti ve yüzey pürüzlülüğü üzerine deneysel çalışma
(Gazi Üniversitesi , Fen Bilimleri Enstitüsü, 2022)
In this study, three Al-12Si-Sr alloys containing different ratios (0.02; 0.1 and 1%) strontium (Sr) were
manufactured by the permanent mold casting method. The microstructures of the manufactured alloys were
determined ...
A performance comparison study of uncoated and TiAlN coated carbide end mill on machining of the Al-35Zn alloy
(Iop Publishing Ltd, 2018)
In this study, Al-35Zn alloy was produced by permanent mold casting. To investigate the cutting performance of uncoated and TiAlN coated carbide end mills on this alloy, a series of tests were carried out in the CNC vertical ...
Zn-15Al-3Cu-1Si alaşımı ve SAE 660 bronzunun yağlı durumdaki aşınma karakteristikleri
(2018)
Bu çalışmada Zn-15Al-3Cu-1Si alaşımının yağlı çalışma koşullarındaki sürtünme ve aşınma davranışlarıblok-disk tipi bir deney düzeneği kullanılarak incelendi. Sürtünme ve aşınma deneyleri farklı yağ debileri(0,25-3,0 cm3h-1), ...
Effect of strontium and magnesium additions on the microstructure and mechanical properties of Al-12Si alloys
(Korean Inst Metals Materials, 2019)
In this study, a binary Al-12Si, eight ternary Al-12Si-Sr, and six quaternary Al-12Si-0.1Sr-(0.2-1)Mg alloys were produced by permanent mold casting. It was observed that microstructure of the binary alloy consisted of the ...
Stronsiyum ve stronsiyum-magnezyum katkılarının ötektiküstü Al-17Si alaşımının içyapı ve mekanik özelliklerine etkisi
(2019)
Al-17Si, Al-17Si-0,1Sr ve Al-17Si-0,1Sr-0,6Mg alaşımları kokil kalıba döküm yöntemi ile üretilmiştir. Alaşımların yapısal ve mekanik özellikleri üretilen alaşım külçelerinden talaşlı imalat yöntemiyle hazırlanan numuneler ...
Bor ile yapılan tane inceltmenin Al-30Zn alaşımının mikroyapı ve mekanik özelliklerine etkisi
(Gazi Univ, Fac Engineering Architecture, 2019)
In this study, one binary aluminum-zinc (Al-30Zn) alloy and nine ternary aluminum-zinc-boron [Al-30Zn-(0.01-2) B] alloys were produced by permanent mold casting method. Structural properties of the produced alloys were ...